Material Notes:
Silicone coated Glass fabric TISOFLON®Information provided by Isoflon.
Physical Properties Metric English Comments
Thickness 530 microns
20.9 mil
Coating Weight 750 g/m²
469 lb/ream
entire thickness; NF EN ISO 2286.2
Mechanical Properties Metric English Comments
Tear Strength 43.0 - 59.0 kN/m
245 - 337 pli
NF EN ISO 1421
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 230 °C
446 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Descriptive Properties Value Comments
Color white or red
Silicone Content (%) 43