Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Jackon JACKOCELL® R211 Expanded Polystyrene Construction and Block Molding

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer Jackon GmbH
Trade Name JACKOCELL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Jackon JACKOCELL® R211 Expanded Polystyrene Construction and Block Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High quality processingHigh strengthLow wasteFast moulding cycles
Physical Properties Metric English Comments
Density 0.0120 - 0.020 g/cc
0.000434 - 0.00072 lb/in³
expanded
Water Absorption 3.65 %
3.65 %
20 g/l; Volume%
3.65 %
3.65 %
16 g/l; Volume%
3.65 %
3.65 %
12 g/l; Volume%
Mechanical Properties Metric English Comments
Flexural Strength 0.135 MPa
19.6 psi
14 g/l
0.195 MPa
28.3 psi
16 g/l
0.220 MPa
31.9 psi
18 g/l
Compressive Strength 0.560 MPa
81.2 psi
12 g/l
0.920 MPa
133 psi
16 g/l
1.22 MPa
177 psi
20 g/l
Thermal Properties Metric English Comments
Thermal Conductivity 0.0350 W/m-K
0.243 BTU-in/hr-ft²-°F
20 g/l; EN 12667
0.0378 W/m-K
0.262 BTU-in/hr-ft²-°F
13.8 g/l; EN 12667
0.0385 W/m-K
0.267 BTU-in/hr-ft²-°F
12 g/l; EN 12667