Material Notes:
Naturally delaminated clay for use in water-based paints and coatings.Industry: Paint & CoatingsUses: Industrial Coatings, E-Coat, PrimerInformation provided by KaMin LLC.
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Bulk Density 0.561 - 0.673 g/cc
0.0203 - 0.0243 lb/in³
Loose
Brightness 87.5 %
87.5 %
Reflectance (TAPPI)
Oil Absorption 40 %
40 %
Fineness >= 5
>= 5
Hegman Grind
Moisture Absorption at Equilibrium <= 1.5 %
<= 1.5 %
As Produced
Particle Size 0.400 µm
0.400 µm
Average Stokes Equivalent Diameter
1.30 µm
1.30 µm
Median (Malvern Laser)
Particle Mesh Size 325 Mesh
325 Mesh
0.005% Retained
pH 5
5
100 g/250 ml H2O Slurry
Specific Surface Area 18.0 m²/g
18.0 m²/g
BET
Descriptive Properties Value Comments
Bulking Value 21.7 lb.gal
CAS Number 1332-58-7
Crystalline Silica (quartz) <0.1%
Physical Form Dry
Shipping Point Macon, GA