Karina 42/55-GE Red Color Concentrate for PVC

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 42/55-GE Red Color Concentrate for PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heavy metal free color concentrate recommended for application in flexible and rigid PVC compounds for general purposes. Recommended use 2%.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.32 - 1.38 g/cc
1.32 - 1.38 g/cc
ASTM D 792
ASTM Color 31.09 - 34.09
31.09 - 34.09
Color B, ME 12
47.69 - 50.69
47.69 - 50.69
Color L, ME 12
52.62 - 55.62
52.62 - 55.62
Color A, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 53 - 57

@Time 15.0 sec
53 - 57

@Time 0.00417 hour
ASTM D 2240
Descriptive Properties Value Comments
Application Extrusion