Karina 550D35/1-AT-IS Ivory PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 550D35/1-AT-IS Ivory PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.15 - 1.19 g/cc
1.15 - 1.19 g/cc
ASTM D 792
ASTM Color -3.18 - 2.82
-3.18 - 2.82
Color A, ME 12
0.68 - 6.68
0.68 - 6.68
Color B, ME 12
79.41 - 85.41
79.41 - 85.41
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 53 - 57

@Time 15.0 sec
53 - 57

@Time 0.00417 hour
NBR 7456
Tensile Strength >= 7.85 MPa
>= 1140 psi
ASTM D 638
Elongation at Break >= 300 %
>= 300 %
ASTM D 638
Descriptive Properties Value Comments
Application Packaging/Stopper Seals