Material Notes:
Flame retardant PVC compound, class 70C (PVC/A), recommended for insulation of electrical wires and cables (BWF).Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.45 - 1.51 g/cc
1.45 - 1.51 g/cc
NBR NM-IEC 60811-1-3
ASTM Color -2.35 - 3.65
-2.35 - 3.65
Color A, ME 12
3.66 - 9.66
3.66 - 9.66
Color B, ME 12
85.06 - 91.06
85.06 - 91.06
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 90 - 94

@Time 15.0 sec
90 - 94

@Time 0.00417 hour
NBR 7456
Tensile Strength >= 12.6 MPa
>= 1820 psi
NBR NM-IEC 60811-1-1
>= 12.6 MPa
>= 1820 psi
After 168H in air oven at 100°C; NBR NM-IEC 60811-1-2
Elongation at Break >= 150 %
>= 150 %
NBR NM-IEC 60811-1-1
>= 150 %
>= 150 %
After 168H in air oven at 100°C; NBR NM-IEC 60811-1-2
Thermal Properties Metric English Comments
Oxygen Index >= 30 %
>= 30 %
NBR 6245
Electrical Properties Metric English Comments
Volume Resistivity >= 3.00e+14 ohm-cm
>= 3.00e+14 ohm-cm
NBR 5403
Descriptive Properties Value Comments
Application General Purpose Profiles
Maximum Variation of Elongation (%) 25