Karina E 02/5-FC-HSF MBU Yellow (OP) Color Concentrate

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 02/5-FC-HSF MBU Yellow (OP) Color Concentrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.81 - 1.87 g/cc
1.81 - 1.87 g/cc
ASTM D 792
Moisture Absorption <= 0.150 %
<= 0.150 %
ME-52
ASTM Color 3.33 - 5.33
3.33 - 5.33
Color A, ME 12
73.01 - 75.01
73.01 - 75.01
Color B, ME 12
79.68 - 81.68
79.68 - 81.68
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 53 - 57

@Time 15.0 sec
53 - 57

@Time 0.00417 hour
ASTM D 2240
Component Elements Properties Metric English Comments
Cadmium, Cd <= 0.0050 %
<= 0.0050 %
IEC 62321
Chromium, Cr <= 0.010 %
<= 0.010 %
IEC 62321
Lead, Pb <= 0.010 %
<= 0.010 %
IEC 62321
Mercury, Hg <= 0.010 %
<= 0.010 %
IEC 62321
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
ASTM D 257
Descriptive Properties Value Comments
Application Blow Molding
Extrusion
Injection
Bromine, Br (%) < 0.01
IEC 62321
Carrier Polymer EVA
Lightfastness 4 to 5
Scale: 1 to 8