Karina E 06/30-FC-LMP Blue Color Concentrate for PVC

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 06/30-FC-LMP Blue Color Concentrate for PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important considerations:Heavy metal freeFormulated with organic and inorganic pigmentsPVC resin based (carrier polymer)Supplied in pellet form and packaged in 25kg bagsRecommended use of 2% to 4%Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.45 - 1.51 g/cc
1.45 - 1.51 g/cc
ASTM D 792
ASTM Color -44.49 - -41.49
-44.49 - -41.49
Color B, ME 12
-9.95 - -6.95
-9.95 - -6.95
Color A, ME 12
43.8 - 46.8
43.8 - 46.8
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 63 - 67

@Time 15.0 sec
63 - 67

@Time 0.00417 hour
ASTM D 2240
Component Elements Properties Metric English Comments
Cadmium, Cd <= 0.0050 %
<= 0.0050 %
IEC 62321
Chromium, Cr <= 0.010 %
<= 0.010 %
IEC 62321
Lead, Pb <= 0.010 %
<= 0.010 %
IEC 62321
Mercury, Hg <= 0.010 %
<= 0.010 %
IEC 62321
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
ASTM D 257
Descriptive Properties Value Comments
Application Extrusion
Injection
Bromine, Br (%) < 0.01
IEC 62321
Pantone Classification (Natural Base) 2945.00C