Karina E 10/85-FC-LMP White Color Concentrate for PVC

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 10/85-FC-LMP White Color Concentrate for PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important considerations:Heavy metal freeFormulated with organic and inorganic pigmentsPVC resin based (carrier polymer)Supplied in pellet form and packaged in 25kg bagsRecommended use of 2% to 4%Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.47 - 1.53 g/cc
1.47 - 1.53 g/cc
NBR NM-IEC 60811-1-3
ASTM Color -2.57 - 0.43
-2.57 - 0.43
Color A, ME 12
1.57 - 4.57
1.57 - 4.57
Color B, ME 12
90.96 - 93.96
90.96 - 93.96
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
NBR 7456
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
NBR 5403
Descriptive Properties Value Comments
Application Extrusion
Injection
RAL Classification (Natural Base) 90.0010.00