Material Notes:
Recommended usage from 2% to 3% on crystal PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.25 - 1.31 g/cc
1.25 - 1.31 g/cc
ASTM D 792
ASTM Color -17.27 - -15.27
-17.27 - -15.27
Color B, ME 12
27.92 - 29.92
27.92 - 29.92
Color A, ME 12
36.25 - 38.25
36.25 - 38.25
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 46 - 50

@Time 15.0 sec
46 - 50

@Time 0.00417 hour
ASTM D 2240