Karina E 42/261-GEN Dark Red MBATCH (SP31543) for PVC

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 42/261-GEN Dark Red MBATCH (SP31543) for PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Recommended usage from 2% to 3% on crystal PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
ASTM D 792
ASTM Color 25.33 - 28.33
25.33 - 28.33
Color B, ME 12
41.56 - 44.56
41.56 - 44.56
Color L, ME 12
46.44 - 49.44
46.44 - 49.44
Color A, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 52 - 56

@Time 15.0 sec
52 - 56

@Time 0.00417 hour
ASTM D 2240
Descriptive Properties Value Comments
Application Extrusion