Karina E 47/35-GI Silver MBATCH for PVC

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 47/35-GI Silver MBATCH for PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Recommended usage from 2% to 3% on crystal PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.44 - 1.50 g/cc
1.44 - 1.50 g/cc
ASTM D 792
ASTM Color -5.61 - 0.39
-5.61 - 0.39
Color B, ME 12
-4.62 - 1.38
-4.62 - 1.38
Color A, ME 12
67.29 - 73.29
67.29 - 73.29
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 65 - 69

@Time 15.0 sec
65 - 69

@Time 0.00417 hour
ASTM D 2240
Descriptive Properties Value Comments
Application Injection