Karina E 754-10/426-AT-IS White PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 754-10/426-AT-IS White PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
White non-toxic PVC compound, recommended for general extrusion.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.20 - 1.26 g/cc
1.20 - 1.26 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 75 - 79

@Time 15.0 sec
75 - 79

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 11.8 MPa
>= 1710 psi
ASTM D 638
Elongation at Break >= 250 %
>= 250 %
ASTM D 638
Descriptive Properties Value Comments
Application General Purpose Profiles