Karina E 800-10/1-AY-RT PVC Compound White Color

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 800-10/1-AY-RT PVC Compound White Color.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.45 - 1.51 g/cc
1.45 - 1.51 g/cc
ASTM D 792
ASTM Color -2.45 - 0.55
-2.45 - 0.55
Color A, ME 12
4.06 - 7.06
4.06 - 7.06
Color B, ME 12
89.04 - 92.04
89.04 - 92.04
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 83 - 87

@Time 15.0 sec
83 - 87

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638