Karina E 847-10/189-IS-SD White PVC Compound

Category Polymer , Film , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 847-10/189-IS-SD White PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
White PVC Compound for extrusion of films/SheetInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.35 - 1.41 g/cc
1.35 - 1.41 g/cc
ASTM D 792
ASTM Color -2.53 - -0.930
-2.53 - -0.930
Color B, ME 12
-1.90 - -0.300
-1.90 - -0.300
Color A, ME 12
92.77 - 94.37
92.77 - 94.37
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Descriptive Properties Value Comments
Application Blister