Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Karina E818-10/23-CRM White PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E818-10/23-CRM White PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.33 - 1.39 g/cc
1.33 - 1.39 g/cc
ASTM D 792
ASTM Color -2.01 - 0.99
-2.01 - 0.99
Color A, ME 12
0.51 - 3.51
0.51 - 3.51
Color B, ME 12
91.05 - 94.05
91.05 - 94.05
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 80

@Time 15.0 sec
78 - 80

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Thermal Properties Metric English Comments
Vicat Softening Point >= 72.0 °C
>= 162 °F
ASTM D 1525
Descriptive Properties Value Comments
Application Fittings
Copyright © lookpolymers.com All Rights Reserved