Karina SDB 40/1-HSF Ivory PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina SDB 40/1-HSF Ivory PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.29 - 1.35 g/cc
1.29 - 1.35 g/cc
NBR NM-IEC 60811-1-3
ASTM Color -2.18 - 0.82
-2.18 - 0.82
Color A, ME 12
5.43 - 8.43
5.43 - 8.43
Color B, ME 12
92.3 - 95.3
92.3 - 95.3
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 38 - 44

@Time 15.0 sec
38 - 44

@Time 0.00417 hour
ASTM D 2240
42 - 48

@Time 15.0 sec
42 - 48

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 19.6 MPa
>= 2840 psi
NBR NM-IEC 60811-1-1
Elongation at Break >= 200 %
>= 200 %
NBR NM-IEC 60811-1-1
Component Elements Properties Metric English Comments
Cadmium, Cd <= 0.0050 %
<= 0.0050 %
IEC 62321
Chromium, Cr <= 0.010 %
<= 0.010 %
IEC 62321
Lead, Pb <= 0.010 %
<= 0.010 %
IEC 62321
Mercury, Hg <= 0.010 %
<= 0.010 %
IEC 62321
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
ASTM D 257
Descriptive Properties Value Comments
Application 90 Grades
Bromine, Br (%) < 0.01
IEC 62321