Karina TR-607D48/1-Y-IS-BZ Black PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina TR-607D48/1-Y-IS-BZ Black PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heavy metal free PVC compound additivated with nitrile rubber.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.17 - 1.23 g/cc
1.17 - 1.23 g/cc
ASTM D 792
ASTM Color -1.10 - 0.50
-1.10 - 0.50
Color B, ME 12
-0.750 - 0.85
-0.750 - 0.85
Color A, ME 12
25.7 - 27.3
25.7 - 27.3
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 58 - 62

@Time 15.0 sec
58 - 62

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Elongation at Break >= 320 %
>= 320 %
ASTM 638
Descriptive Properties Value Comments
Application General Purpose Injection Molded Parts