Material Notes:
Production Method: HDPE is produced by high pressure ethylene polymerization in tubular reactors. Application: Intended for production of bags, pipes, fittings, articles designed for food contact, toys, films and film articles, shaped-molded parts, etc.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
Density 0.917 - 0.919 g/cc
0.0331 - 0.0332 lb/in³
Melt Flow 7.0 g/10 min
7.0 g/10 min
±15%
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 9.30 MPa
>= 1350 psi
Elongation at Break >= 450 %
>= 450 %
Tear Strength Test >= 9.8
>= 9.8
MPa
Descriptive Properties Value Comments
Amount of impurities [pcs] 10
2nd Quality
2
Superior Quality
5
Premium Quality
Extractable Substance Weight Content (%) 1.2