Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kazanorgsintez PE2NT26-13 High Density Polyethylene Composite

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Kazanorgsintez
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kazanorgsintez PE2NT26-13 High Density Polyethylene Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended for injection molding processing into goods for household and domestic use or for other field of application and characterized by advanced crack resistance.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
Density 0.948 - 0.955 g/cc

@Temperature 23.0 °C
0.0342 - 0.0345 lb/in³

@Temperature 73.4 °F
0.950 - 0.957 g/cc

@Temperature 20.0 °C
0.0343 - 0.0346 lb/in³

@Temperature 68.0 °F
Environmental Stress Crack Resistance >= 50 hour
>= 50 hour
Melt Flow 0.80 - 1.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
±15%
16 - 56 g/10 min

@Load 21.6 kg,
Temperature 190 °C
16 - 56 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Elongation at Break >= 750 %
>= 750 %
Descriptive Properties Value Comments
Amount of impurities [pcs] 10