Kennametal Stellite Delcrome 6272 Iron Alloy

Category Metal , Ferrous Metal , Superalloy
Manufacturer Kennametal Stellite
Trade Name Delcrome
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Delcrome 6272 Iron Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Corrosion resistant alloys with moderate to high metal to metal wear resistance.Information provided by Kennametal Stelliteâ„¢
Mechanical Properties Metric English Comments
Hardness, Rockwell C 44
44
Component Elements Properties Metric English Comments
Carbon, C <= 14 %
<= 14 %
Chromium, Cr 25 %
25 %
Iron, Fe >= 27.2 %
>= 27.2 %
as balance
Molybdenum, Mo 7.0 %
7.0 %
Silicon, Si 1.8 %
1.8 %
Tungsten, W <= 25 %
<= 25 %
Descriptive Properties Value Comments
Application Technique PTA & laser deposition