Material Notes:
An alloy developed by EPRI (Electrical Power Research Institute) for use in Nuclear valve application.Information provided by Kennametal Stelliteâ„¢
Mechanical Properties Metric English Comments
Hardness, Rockwell C 40
40
Component Elements Properties Metric English Comments
Carbon, C <= 4.0 %
<= 4.0 %
Chromium, Cr 25 %
25 %
Iron, Fe >= 59.85 %
>= 59.85 %
as balance
Manganese, Mn 4.5 %
4.5 %
Molybdenum, Mo 2.0 %
2.0 %
Silicon, Si 3.4 %
3.4 %
Tungsten, W <= 1.25 %
<= 1.25 %
Descriptive Properties Value Comments
Application Technique PTA & laser deposition