Material Notes:
Applications: include vane plugs, fuel metering pins, spacer bushings, ball blanks (bearings), race blanks (bearings), diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous wear parts.Data provided by the manufacturer, Deloro Stellite Inc.Product of former Deloro Stellite Inc.
Physical Properties Metric English Comments
Density 8.28 g/cc
0.299 lb/in³
P/M (97%), 8.52 g/cc theoretical.
Mechanical Properties Metric English Comments
Hardness, Brinell 404
404
Converted from Rockwell C hardness.
Hardness, Knoop 486
486
Converted from Rockwell C hardness.
Hardness, Rockwell A 72
72
Converted from Rockwell C hardness.
Hardness, Rockwell B 113
113
Converted from Rockwell C hardness. Beyond normal Rockwell B range, for comparison only.
Hardness, Rockwell C 44
44
Hot hardness.
Hardness, Vickers 428
428
Converted from Rockwell C hardness.
Thermal Properties Metric English Comments
CTE, linear 11.9 µm/m-°C

@Temperature 0.000 - 100 °C
6.61 µin/in-°F

@Temperature 32.0 - 212 °F
12.8 µm/m-°C

@Temperature 0.000 - 200 °C
7.11 µin/in-°F

@Temperature 32.0 - 392 °F
12.9 µm/m-°C

@Temperature 0.000 - 300 °C
7.17 µin/in-°F

@Temperature 32.0 - 572 °F
13.4 µm/m-°C

@Temperature 0.000 - 400 °C
7.44 µin/in-°F

@Temperature 32.0 - 752 °F
13.8 µm/m-°C

@Temperature 0.000 - 500 °C
7.67 µin/in-°F

@Temperature 32.0 - 932 °F
14.1 µm/m-°C

@Temperature 0.000 - 600 °C
7.83 µin/in-°F

@Temperature 32.0 - 1110 °F
14.4 µm/m-°C

@Temperature 0.000 - 700 °C
8.00 µin/in-°F

@Temperature 32.0 - 1290 °F
15.2 µm/m-°C

@Temperature 0.000 - 800 °C
8.44 µin/in-°F

@Temperature 32.0 - 1470 °F
15.5 µm/m-°C

@Temperature 0.000 - 900 °C
8.61 µin/in-°F

@Temperature 32.0 - 1650 °F
15.8 µm/m-°C

@Temperature 0.000 - 1000 °C
8.78 µin/in-°F

@Temperature 32.0 - 1830 °F
Melting Point 1255 - 1341 °C
2291 - 2446 °F
Solidus 1255 °C
2291 °F
Liquidus 1341 °C
2446 °F
Component Elements Properties Metric English Comments
Boron, B 1.0 %
1.0 %
Carbon, C 1.5 %
1.5 %
Chromium, Cr 30 %
30 %
Cobalt, Co 48 %
48 %
As remainder
Iron, Fe <= 3.0 %
<= 3.0 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Nickel, Ni <= 3.0 %
<= 3.0 %
Other <= 3.0 %
<= 3.0 %
Silicon, Si <= 1.0 %
<= 1.0 %
Tungsten, W 8.5 %
8.5 %
Electrical Properties Metric English Comments
Magnetic Permeability <= 1.20

@Temperature 22.0 °C
<= 1.20

@Temperature 71.6 °F
200 Oersted
Copyright © lookpolymers.com All Rights Reserved