Kennametal Stellite Stellite® 6K 12.7 or 22.2 mm plate

Category Metal , Nonferrous Metal , Cobalt Alloy , Superalloy
Manufacturer Kennametal Stellite
Trade Name Stellite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Stellite® 6K 12.7 or 22.2 mm plate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
13.3 mm^3 volume loss--abrasive wear data. Applications include agitators, augers, ball mills, banbury mills, cams, crusher bearings, dryers, dry presses, dump cars, fans, filters, food machinery, galvanizing roll necks, grinder ring bearings, marine equipment, mixing equipment, pulleys, pump seals, pump shafts, rotary kilns, scraper rolls, screw conveyors, spindles, stuffing boxes, thickeners, tile presses, wear bars. Data provided by the manufacturer, Deloro Stellite Inc.Product of former Deloro Stellite Inc.
Physical Properties Metric English Comments
Density 8.387 g/cc
0.3030 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1008 MPa
146200 psi
729 MPa

@Temperature 538 °C
106000 psi

@Temperature 1000 °F
785 MPa

@Temperature 316 °C
114000 psi

@Temperature 600 °F
Tensile Strength, Yield 746 MPa

@Strain 0.200 %
108000 psi

@Strain 0.200 %
517 MPa

@Strain 0.200 %,
Temperature 538 °C
75000 psi

@Strain 0.200 %,
Temperature 1000 °F
555 MPa

@Strain 0.200 %,
Temperature 316 °C
80500 psi

@Strain 0.200 %,
Temperature 600 °F
Elongation at Break 1.0 %
1.0 %
in 25.4 mm
2.0 %

@Temperature 316 °C
2.0 %

@Temperature 600 °F
in 25.4 mm
3.0 %

@Temperature 538 °C
3.0 %

@Temperature 1000 °F
in 25.4 mm
Thermal Properties Metric English Comments
CTE, linear 13.8 µm/m-°C

@Temperature 0.000 - 100 °C
7.67 µin/in-°F

@Temperature 32.0 - 212 °F
13.8 µm/m-°C

@Temperature 0.000 - 300 °C
7.67 µin/in-°F

@Temperature 32.0 - 572 °F
13.8 µm/m-°C

@Temperature 0.000 - 400 °C
7.67 µin/in-°F

@Temperature 32.0 - 752 °F
13.8 µm/m-°C

@Temperature 0.000 - 200 °C
7.67 µin/in-°F

@Temperature 32.0 - 392 °F
14.0 µm/m-°C

@Temperature 0.000 - 600 °C
7.78 µin/in-°F

@Temperature 32.0 - 1110 °F
14.2 µm/m-°C

@Temperature 0.000 - 700 °C
7.89 µin/in-°F

@Temperature 32.0 - 1290 °F
14.5 µm/m-°C

@Temperature 0.000 - 800 °C
8.06 µin/in-°F

@Temperature 32.0 - 1470 °F
14.9 µm/m-°C

@Temperature 0.000 - 900 °C
8.28 µin/in-°F

@Temperature 32.0 - 1650 °F
15.5 µm/m-°C

@Temperature 0.000 - 1000 °C
8.61 µin/in-°F

@Temperature 32.0 - 1830 °F
Melting Point 1265 - 1354 °C
2309 - 2469 °F
Solidus 1265 °C
2309 °F
Liquidus 1354 °C
2469 °F
Component Elements Properties Metric English Comments
Carbon, C 1.4 - 1.9 %
1.4 - 1.9 %
Chromium, Cr 28 - 32 %
28 - 32 %
Cobalt, Co 49.1 - 55.6 %
49.1 - 55.6 %
As remainder
Iron, Fe <= 3.0 %
<= 3.0 %
Manganese, Mn <= 2.0 %
<= 2.0 %
Molybdenum, Mo <= 1.5 %
<= 1.5 %
Nickel, Ni <= 3.0 %
<= 3.0 %
Silicon, Si <= 2.0 %
<= 2.0 %
Tungsten, W 3.5 - 5.5 %
3.5 - 5.5 %
Electrical Properties Metric English Comments
Magnetic Permeability <= 1.20

@Temperature 22.0 °C
<= 1.20

@Temperature 71.6 °F
200 Oersted (15.900 A/m)