Adhesive wear test data P/M 0.58 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous wear parts. Data provided by the manufacturer, Deloro Stellite, Inc.Product of former Deloro Stellite Inc.
Physical Properties Metric English Comments
Density 8.45 g/cc
0.305 lb/in³
P/M (98%)
8.63 g/cc
0.312 lb/in³
Theoretical
Mechanical Properties Metric English Comments
Hardness, Rockwell C 58
58
Hot hardness.
Tensile Strength, Ultimate 794 MPa
115000 psi
656 MPa

@Temperature 760 °C
95100 psi

@Temperature 1400 °F
690 MPa

@Temperature 649 °C
100000 psi

@Temperature 1200 °F
725 MPa

@Temperature 538 °C
105000 psi

@Temperature 1000 °F
Elongation at Break 0.30 %
0.30 %
in 25.4 mm
0.30 %

@Temperature 538 °C
0.30 %

@Temperature 1000 °F
in 25.4 mm
0.50 %

@Temperature 649 °C
0.50 %

@Temperature 1200 °F
in 25.4 mm
0.50 %

@Temperature 760 °C
0.50 %

@Temperature 1400 °F
in 25.4 mm
Thermal Properties Metric English Comments
CTE, linear 10.8 µm/m-°C

@Temperature 20.0 - 100 °C
6.00 µin/in-°F

@Temperature 68.0 - 212 °F
11.1 µm/m-°C

@Temperature 20.0 - 200 °C
6.17 µin/in-°F

@Temperature 68.0 - 392 °F
11.5 µm/m-°C

@Temperature 20.0 - 300 °C
6.39 µin/in-°F

@Temperature 68.0 - 572 °F
11.7 µm/m-°C

@Temperature 20.0 - 400 °C
6.50 µin/in-°F

@Temperature 68.0 - 752 °F
12.1 µm/m-°C

@Temperature 20.0 - 500 °C
6.72 µin/in-°F

@Temperature 68.0 - 932 °F
12.7 µm/m-°C

@Temperature 20.0 - 600 °C
7.06 µin/in-°F

@Temperature 68.0 - 1110 °F
13.0 µm/m-°C

@Temperature 20.0 - 700 °C
7.22 µin/in-°F

@Temperature 68.0 - 1290 °F
13.4 µm/m-°C

@Temperature 20.0 - 800 °C
7.44 µin/in-°F

@Temperature 68.0 - 1470 °F
13.7 µm/m-°C

@Temperature 20.0 - 900 °C
7.61 µin/in-°F

@Temperature 68.0 - 1650 °F
14.1 µm/m-°C

@Temperature 20.0 - 1000 °C
7.83 µin/in-°F

@Temperature 68.0 - 1830 °F
Melting Point 1224 - 1275 °C
2235 - 2327 °F
Solidus 1224 °C
2235 °F
Liquidus 1275 °C
2327 °F
Component Elements Properties Metric English Comments
Boron, B 1.0 %
1.0 %
Carbon, C 2.0 %
2.0 %
Chromium, Cr 30 %
30 %
Cobalt, Co 31 %
31 %
As remainder
Iron, Fe <= 5.0 %
<= 5.0 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Molybdenum, Mo <= 0.80 %
<= 0.80 %
Nickel, Ni 3.5 %
3.5 %
Other <= 2.0 %
<= 2.0 %
Silicon, Si <= 1.0 %
<= 1.0 %
Tungsten, W 18.5 %
18.5 %
Vanadium, V 4.2 %
4.2 %
Electrical Properties Metric English Comments
Magnetic Permeability <= 1.20

@Temperature 22.0 °C
<= 1.20

@Temperature 71.6 °F
116 Oersted