Kinetics MIM 2.5% SiFe Soft Magnetic Steel

Category Metal , Electronic/Magnetic Alloy , Ferrous Metal
Manufacturer Kinetics, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kinetics MIM 2.5% SiFe Soft Magnetic Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low alloy steel, silicon. A work hardenable steel alloy that offers very good magnetic properties, tensile strength, hardness, wear resistance, and increased spring steel strength. Can be plated or coated for corrosion resistance. Often used for armatures, relays, solenoids, and applications where good magnetic, low core loss and high electrical resistivity in AC and DC applications is required.Property values reported are typical for Kinetics' MIM products.Metal Injection Molding General Notes: Fine metal powders (generally
Physical Properties Metric English Comments
Density 7.61 g/cc
0.275 lb/in³
Sintered
Mechanical Properties Metric English Comments
Hardness, Rockwell B 82
82
Tensile Strength, Ultimate 483 MPa
70000 psi
Tensile Strength, Yield 338 MPa
49000 psi
Elongation at Break 24 %
24 %
in 1 inch
Reduction of Area 43 %
43 %
Charpy Impact, Unnotched 213 J
157 ft-lb
1/2 size bar
Component Elements Properties Metric English Comments
Carbon, C <= 0.060 %
<= 0.060 %
Iron, Fe 97.19 - 97.85 %
97.19 - 97.85 %
Iron content calculated by difference.
Silicon, Si 2.15 - 2.75 %
2.15 - 2.75 %
Descriptive Properties Value Comments
Surface Finish 24 Ra