Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kingfa PET-RG15 Flame Retardant, 15% Glass Fiber Reinforced PET

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
Manufacturer Kingfa Sci. & Tech. Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kingfa PET-RG15 Flame Retardant, 15% Glass Fiber Reinforced PET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Flame retardantHigh strengthGood heat resistanceOutstanding electrical propertiesApplications:Injection moldingConnectorsRelayBobbinsSocketsE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.55 g/cc

@Temperature 23.0 °C
1.55 g/cc

@Temperature 73.4 °F
ASTM D792
Water Absorption 0.070 %

@Temperature 23.0 °C,
Time 86400 sec
0.070 %

@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0050 - 0.011 cm/cm

@Temperature 23.0 °C
0.0050 - 0.011 in/in

@Temperature 73.4 °F
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength at Break 105 MPa
15200 psi
10mm/min; ASTM D638
Elongation at Break 2.6 %
2.6 %
10mm/min; ASTM D638
Flexural Strength 170 MPa
24700 psi
2mm/min; ASTM D790
Flexural Modulus 7.00 GPa
1020 ksi
2mm/min; ASTM D790
Izod Impact, Notched 0.700 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
1.31 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 230 °C

@Thickness 6.40 mm
446 °F

@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 215 °C

@Thickness 6.40 mm
419 °F

@Thickness 0.252 in
ASTM D648
Flammability, UL94 V-0

@Thickness 0.750 mm
V-0

@Thickness 0.0295 in
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Processing Temperature <= 270 °C
<= 518 °F
Rear Barrel Temperature 235 - 255 °C
455 - 491 °F
Start Point: 245°C
Middle Barrel Temperature 245 - 265 °C
473 - 509 °F
Start Point: 250°C
Front Barrel Temperature 255 - 275 °C
491 - 527 °F
Start Point: 260°C
Melt Temperature 255 - 275 °C
491 - 527 °F
Start Point: 260°C
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Start Point: 100°C
Drying Temperature 120 - 140 °C

@Time 10800 - 18000 sec
248 - 284 °F

@Time 3.00 - 5.00 hour
Pre-dry
Descriptive Properties Value Comments
Glass Fiber Content (%) 15
Injection Speed Moderate to High