Material Notes:
Class I/A rated thermoplastic sheetApplications: Interior ductwork and chutes, laboratory hoods, shower/tub shrouds, acoustical applications, decorative ceilings, abuse resistant surfacing for counters, exhibits, partitions, doorsFeatures: Kydex 160 sheet is more resistant to a wider range of concentrated chemicals than any other thermoplastic. Its superior chemical resistance allows for excellent cleanability because stronger clearing agents can be sued with no discoloration or surface damage to the material. Fabrication: Kydex 160 has good formability and extensibility a and is extremely easy to work with once formed.Data provided by the Kleerdex Company.Kleerdex Company became KYDEX, LLC in 2009.
Physical Properties Metric English Comments
Density 1.35 - 1.45 g/cc
0.0488 - 0.0524 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D785
Tensile Strength, Ultimate 40.0 MPa
5800 psi
ASTM D638
Elongation at Break 70 %
70 %
Modulus of Elasticity 2.557 GPa
370.9 ksi
Flexural Yield Strength 72.0 MPa
10400 psi
ASTM D790
Izod Impact, Notched 1.07 - 2.14 J/cm

@Temperature 23.0 °C
2.00 - 4.01 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
annealed; ASTM D648