Kobe Steel KS EL-F Alpha-Beta Titanium Alloy, Annealed

Category Metal , Nonferrous Metal , Titanium Alloy
Manufacturer Kobe Steel
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kobe Steel KS EL-F Alpha-Beta Titanium Alloy, Annealed.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nominal Composition: Ti-4.5 Al-4 Cr-0.5 Fe-0.2 C Applications: Aircraft parts, connecting rods, valve spring retainers, structural parts, golf club heads.Features:High strength, excellent balance between strength and toughness.Information provided by Kobe Steel
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 895 MPa
>= 130000 psi
Tensile Strength, Yield >= 828 MPa
>= 120000 psi
0.2% proof
Elongation at Break >= 10 %
>= 10 %
Reduction of Area >= 20 %
>= 20 %
Component Elements Properties Metric English Comments
Aluminum, Al 4.0 - 5.0 %
4.0 - 5.0 %
Carbon, C 0.080 - 0.25 %
0.080 - 0.25 %
Chromium, Cr 3.5 - 4.5 %
3.5 - 4.5 %
Hydrogen, H <= 0.015 %
<= 0.015 %
Iron, Fe 0.20 - 0.80 %
0.20 - 0.80 %
Nitrogen, N <= 0.050 %
<= 0.050 %
Oxygen, O <= 0.25 %
<= 0.25 %
Titanium, Ti >= 89.135 %
>= 89.135 %
As Remainder