Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kobe Steel KS6-4 Alpha-Beta Titanium Alloy, ASTM Gr. 5, Annealed

Category Metal , Nonferrous Metal , Titanium Alloy
Manufacturer Kobe Steel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kobe Steel KS6-4 Alpha-Beta Titanium Alloy, ASTM Gr. 5, Annealed.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nominal Composition: Ti-6 Al-4 V Applications: Aircraft parts, connecting rods, valve spring retainers, structural parts, golf club heads.Features:High strength, excellent balance between strength and toughness.Information provided by Kobe Steel
Physical Properties Metric English Comments
Density 4.43 g/cc
0.160 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 895 MPa
>= 130000 psi
Tensile Strength, Yield >= 828 MPa
>= 120000 psi
0.2% proof
Elongation at Break >= 10 %
>= 10 %
Reduction of Area >= 25 %
>= 25 %
Bend Radius, Minimum 4.5 t
4.5 t
t ≤ 1.8 mm
5.0 t
5.0 t
1.8 < t ≤ 4.75 mm
Component Elements Properties Metric English Comments
Aluminum, Al 5.5 - 6.75 %
5.5 - 6.75 %
Carbon, C <= 0.080 %
<= 0.080 %
Hydrogen, H <= 0.015 %
<= 0.015 %
Iron, Fe <= 0.40 %
<= 0.40 %
Nitrogen, N <= 0.050 %
<= 0.050 %
Oxygen, O <= 0.20 %
<= 0.20 %
Titanium, Ti >= 88.005 %
>= 88.005 %
As Remainder
Vanadium, V 3.5 - 4.5 %
3.5 - 4.5 %
Users viewing this material also viewed the following: