Kobe Steel KSG12 Titanium alloy with low alloying elements, ASTM Gr. 12, Annealed

Category Metal , Nonferrous Metal , Titanium Alloy
Manufacturer Kobe Steel
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kobe Steel KSG12 Titanium alloy with low alloying elements, ASTM Gr. 12, Annealed.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nominal Composition: Ti-0.3 Mo-0.8 Ni Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant. Information provided by Kobe Steel
Physical Properties Metric English Comments
Density 4.50 g/cc
0.163 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 483 MPa
>= 70100 psi
Tensile Strength, Yield >= 345 MPa
>= 50000 psi
0.2% proof
Elongation at Break >= 18 %
>= 18 %
Reduction of Area >= 25 %
>= 25 %
Bend Radius, Minimum 2.0 t
2.0 t
t ≤ 1.8 mm
2.5 t
2.5 t
1.8 < t ≤ 4.75 mm
Component Elements Properties Metric English Comments
Carbon, C <= 0.080 %
<= 0.080 %
Hydrogen, H <= 0.015 %
<= 0.015 %
Iron, Fe <= 0.30 %
<= 0.30 %
Molybdenum, Mo 0.20 - 0.40 %
0.20 - 0.40 %
Nickel, Ni 0.60 - 0.90 %
0.60 - 0.90 %
Nitrogen, N <= 0.030 %
<= 0.030 %
Oxygen, O <= 0.25 %
<= 0.25 %
Titanium, Ti >= 98.025 %
>= 98.025 %
As Remainder