Kolon ELLAS K-395F Ether Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Kolon
Trade Name ELLAS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon ELLAS K-395F Ether Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsExtrusionHighly Pressurized Hose Information provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 95
95
ASTM D2240
Tensile Strength 45.1 MPa
6540 psi
ASTM D412
Tensile Stress 11.8 MPa

@Strain 100 %
1710 psi

@Strain 100 %
ASTM D412
Elongation at Break 500 %
500 %
ASTM D412
Tear Strength 137 kN/m
784 pli
ASTM D624
Processing Properties Metric English Comments
Nozzle Temperature 175 - 185 °C
347 - 365 °F
Injection Molding
Zone 1 150 - 160 °C
302 - 320 °F
Injection Molding
155 - 175 °C
311 - 347 °F
Extrusion Molding
Zone 2 160 - 170 °C
320 - 338 °F
Injection Molding
170 - 185 °C
338 - 365 °F
Extrusion Molding
Zone 3 170 - 180 °C
338 - 356 °F
Injection Molding
170 - 190 °C
338 - 374 °F
Extrusion Molding
Zone 4 180 - 195 °C
356 - 383 °F
Extrusion Molding
Die Temperature 180 - 195 °C
356 - 383 °F
Extrusion Molding
Head Temperature 190 - 200 °C
374 - 392 °F
Extrusion Molding