Flexible grade. Applications: Flexible products. Information provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Melt Flow 8.0 - 11 g/10 min
8.0 - 11 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 70
70
ASTM D785
Tensile Strength 29.0 MPa
4210 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Strength 41.0 MPa
5950 psi
ASTM D790
Flexural Modulus 1.088 GPa
157.8 ksi
ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 166 °C
331 °F
ASTM D1525
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D257
Users viewing this material also viewed the following: