Kolon KOCETAL® GF702 G/F Reinforced Acetal Resin

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, 10% Glass Fiber Reinforced
Manufacturer Kolon
Trade Name Kocetal®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon KOCETAL® GF702 G/F Reinforced Acetal Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass fiber reinforced, improved stiffness. Applications: Products for high stiffness, improved fatigue properties. Information provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D792
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
Melt Flow 15 - 20 g/10 min
15 - 20 g/10 min
ASTM D1238
Ash 8.0 - 12 %
8.0 - 12 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 85
85
ASTM D785
Tensile Strength 74.0 MPa
10700 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Flexural Strength 118 MPa
17100 psi
ASTM D790
Flexural Modulus 4.413 GPa
640.1 ksi
ASTM D790
Izod Impact, Notched 0.290 J/cm
0.543 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 166 °C
331 °F
ASTM D1525
Deflection Temperature at 0.46 MPa (66 psi) 165 °C
329 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D257