Kolon KOCETAL® LF302 Wear Modified Acetal Resin

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer Kolon
Trade Name Kocetal®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon KOCETAL® LF302 Wear Modified Acetal Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Improved wear property and dimensional stability. Applications: Products for low noise and precision gear. Information provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Linear Mold Shrinkage 0.018 cm/cm
0.018 in/in
ASTM D955
Melt Flow 7.0 - 10 g/10 min
7.0 - 10 g/10 min
ASTM D1238
Ash 8.0 - 12 %
8.0 - 12 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 80
80
ASTM D785
Tensile Strength 50.0 MPa
7250 psi
ASTM D638
Elongation at Break 39 %
39 %
ASTM D638
Flexural Strength 83.0 MPa
12000 psi
ASTM D790
Flexural Modulus 2.158 GPa
313.0 ksi
ASTM D790
Izod Impact, Notched 0.910 J/cm
1.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 166 °C
331 °F
ASTM D1525
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D257