Material Notes:
Whisker reinforced, improved wear and dimensional property. Applications: Dimensionally precise products. Information provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.55 g/cc
1.55 g/cc
ASTM D792
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Melt Flow 18 - 23 g/10 min
18 - 23 g/10 min
ASTM D1238
Ash 18 - 22 %
18 - 22 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 85
85
ASTM D785
Tensile Strength 44.0 MPa
6380 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 83.0 MPa
12000 psi
ASTM D790
Flexural Modulus 4.41 GPa
640 ksi
ASTM D790
Izod Impact, Notched 0.200 J/cm
0.375 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 166 °C
331 °F
ASTM D1525
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D257