Kolon KOPA® KN3321G10V0L G/F Reinforced & Flame Retardant Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Fiber Filled, Flame Retardant
Manufacturer Kolon
Trade Name Kopa®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon KOPA® KN3321G10V0L G/F Reinforced & Flame Retardant Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High flame resistant, high toughness, dimensionally stableApplications A variety of connectorsInformation provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.70 %
0.70 %
60% RH; ASTM D570
Linear Mold Shrinkage 0.0050 - 0.010 cm/cm
0.0050 - 0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength 89.0 MPa
12900 psi
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
Flexural Strength 143 MPa
20700 psi
ASTM D790
Flexural Modulus 4.806 GPa
697.1 ksi
ASTM D790
Izod Impact, Notched 0.740 J/cm
1.39 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C
16.7 µin/in-°F
ASTM D696
Melting Point 255 °C
491 °F
ASTM D1525
Deflection Temperature at 0.46 MPa (66 psi) 240 °C
464 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 235 °C
455 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 3.6
3.6
ASTM D150
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149
Arc Resistance 130 sec
130 sec
ASTM D495