Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kraiburg TPE THERMOLAST® K TC4FRN Thermoplastic Elastomer, Flame retardant  (Unverified Data**)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraiburg TPE THERMOLAST® K TC4FRN Thermoplastic Elastomer, Flame retardant  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Markets / Application Sectors:Electrics & ElectronicsApplication Examples:Injection molding parts for electric equipmentElectric plugsElectric grommetsSwitchboxesCable distributorsMaterial Advantages:Excellent physical propertiesHalogen free (corroding or corrosive fire gases as well as a subsequent dioxin contamination can thereby be avoided)Flame retardantTested acc. UL 94-V0Self-extinguishing, low smoke emission and no dripping of flaming particlesEasy to colorSound absorbingInformation Provided by Kraiburg TPE Corp.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
DIN EN ISO 1183-1:2004
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
DIN 53505 / ISO 868
Tensile Strength at Break 2.50 MPa
363 psi
Deviating from ISO 37 standard test piece S2 is tested with a traverse speed of 200 mm/min; DIN 53504 / ISO 37
Elongation at Break 520 %
520 %
Deviating from ISO 37 standard test piece S2 is tested with a traverse speed of 200 mm/min; DIN 53504 / ISO 37
Graves Tear Strength 12.0 kN/m
68.5 pli
DIN ISO 34-1 Method B (b)
Compression Set 7.0 %

@Temperature 23.0 °C,
Time 259000 sec
7.0 %

@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
34 %

@Temperature 70.0 °C,
Time 79200 sec
34 %

@Temperature 158 °F,
Time 22.0 hour
ISO 815
81 %

@Temperature 100 °C,
Time 79200 sec
81 %

@Temperature 212 °F,
Time 22.0 hour
ISO 815
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Processing Temperature 180 - 220 °C
356 - 428 °F
Drying Temperature 80.0 °C

@Time 7200 sec
176 °F

@Time 2.00 hour
Pre drying
Descriptive Properties Value Comments