Material Notes:
Description: Kraton A1536 H is a linear triblock copolymer based on styrene and ethylene/butylene. It is supplied from North America in the physical form identified: Kraton A1536 HU - supplied to customers as an undusted powderKraton A1536 HS - supplied to customers as a dusted powderRegion: Asia Pacific, Europe, Japan, North America, and South AmericaUses: Kraton A1536 H is used in compound formulations and as a modifier of thermoplastics. It may also find use in formulating adhesives, sealants, coatings and modified bitumens.Applications: Compounding and Personal HygieneInformation provided by Kraton®
Physical Properties Metric English Comments
Volatiles <= 1.0 %
<= 1.0 %
KM 04
Melt Flow 7.0 g/10 min

@Load 5.00 kg,
Temperature 260 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Ash 0.35 - 0.70 %
0.35 - 0.70 %
Silica dusted; BAM 908
Mechanical Properties Metric English Comments
Hardness, Shore A 65

@Time 10.0 sec
65

@Time 0.00278 hour
Measured on compression molded slabs; ASTM D2240
Tensile Strength >= 34.5 MPa
>= 5000 psi
Measured on solution cast film from toluene; BAM 1245
Elongation at Break >= 660 %
>= 660 %
Measured on solution cast film from toluene; BAM 1245
300% Modulus 0.00645 GPa
0.936 ksi
Measured on solution cast film from toluene; BAM 1245
Descriptive Properties Value Comments
Content Non-staining phenolic antioxidant
0.07-0.13%, KM 08
Polystyrene
37-44%, Measured on the polymer before hydrogenation, KM 03
Total Extractables
<1.6%, KM 05