Kraton® D1101 A (SBS) Liner Block Copolymer

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Kraton
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® D1101 A (SBS) Liner Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Kraton D1101 A polymer is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Europe in the physical forms identified as follows in the grade nomenclature:D1101 AT - supplied as porous pellets dusted with talcD1101 AS - supplied as porous pellets dusted with amorphous silicaD1101 ASM - supplied as powder dusted with amorphous silicaD1101 AIM - supplied as powder dusted with calcium carbonate for supply to the North American marketD1101 AU - supplied as porous pellets undustedRegion: Asia Pacific, Europe, Japan, North America and South AmericaUses: Kraton D1101 A polymer is used as a modifier of bitumen in roofing felt compounds, roads and pipe coating. It may also be suitable for use in formulating adhesives, sealants and coatings and in the modification of polymers.Applications: Bitumen Modification; Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and RoofingInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 2781
Bulk Density 0.400 g/cc
0.0145 lb/in³
ASTM D 1895 method B
Volatiles <= 0.30 %
<= 0.30 %
KM 04
Viscosity 3000 - 5000 cP
3000 - 5000 cP
25% Toluene Solution at 25°C; KM 06
Melt Flow <= 1.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
<= 1.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Ash <= 0.20 %
<= 0.20 %
AU; ISO 247
<= 0.40 %
<= 0.40 %
AS; ISO 247
<= 0.40 %
<= 0.40 %
AT; ISO 247
2.5 - 4.5 %
2.5 - 4.5 %
AIM; BAM 908
2.5 - 5.0 %
2.5 - 5.0 %
ASM; ISO 247
Mechanical Properties Metric English Comments
Hardness, Shore A 72

@Time 10.0 sec
72

@Time 0.00278 hour
Measure on compression molded slabs; ISO 868
Tensile Strength 33.0 MPa
4790 psi
measured on films cast from a solution in toluene; ISO 37
Elongation at Break 880 %
880 %
Measured on films cast from a solution in toluene; ISO 37
300% Modulus 0.00290 GPa
0.421 ksi
measured on films cast from a solution in toluene; ISO 37
Descriptive Properties Value Comments
Content Antioxidant
>0.14%, KM 08
Polystyrene
30-32%, KM 03
Total Extractables
<1.0%, KM 05