Kraton® D1101 J (SBS) Liner Block Copolymer

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Kraton
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® D1101 J (SBS) Liner Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Kraton D1101 J is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Japan in the physical form(s) outlined in the following grade nomenclature:D1101 JO - supplied as dusted crumbD1101 JU - supplied as undusted crumbD1101 JSM - supplied as powder dusted with amorphous silicaRegion: Asia Pacific, Europe, Japan, North America and South AmericaUses: Kraton D1101 J is used as a modifier of bitumen and polymers. It is also suitable as an ingredient in formulating compounds for footwear applications and may be used in formulating adhesives, sealants and coatings.Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; and Roads and RoofingInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
Volatiles <= 1.0 %

@Temperature 110 °C,
Time 7200 sec
<= 1.0 %

@Temperature 230 °F,
Time 2.00 hour
Viscosity 3000 - 5000 cP
3000 - 5000 cP
25% Toluene Solution at 25°C; KM 06
Melt Flow <= 1.0 g/10 min
<= 1.0 g/10 min
ISO 37
Ash >= 0.50 %
>= 0.50 %
JU; ISO 247
>= 1.0 %
>= 1.0 %
JO; ISO 247
>= 5.0 %
>= 5.0 %
JSM; ISO 247
Mechanical Properties Metric English Comments
Hardness, Shore A 72

@Time 30.0 sec
72

@Time 0.00833 hour
ISO 868
Tensile Strength 33.0 MPa
4790 psi
ISO 37
300% Modulus 0.00290 GPa
0.421 ksi
ISO 37
Descriptive Properties Value Comments
Content Bound Styrene
31 percent