Material Notes:
Description: Kraton D1116 E is a clear, radial triblock copolymer based on styrene and butadiene with a polystyrene content of 23%. It is supplied from Europe in the physical form identified: Kraton D1116 ES - supplied as porous pellets dusted with an amorphous silicaKraton D1116 ESM - supplied as powder dusted with an amorphous silicaRegion: Asia Pacific, Europe, Japan, North America, and South America Uses: Kraton D1116 E is used as a modifier of bitumen and polymers. It is also suitable as an ingredient in formulating compounds for footwear applications and may be used in formulating adhesives, sealants, and coatings. Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and RoofingInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 2781
Volatiles <= 0.30 %
<= 0.30 %
KM 04
Viscosity 2000 - 3000 cP
2000 - 3000 cP
25% Toluene Solution at 25°C; KM 06
Ash <= 0.35 %
<= 0.35 %
ES; ISO 247
Descriptive Properties Value Comments
Content Antioxidant
>0.14%, KM 08
Polystyrene
21.5-24.1%, KM 03
Total Extractables
<1.0%, KM 05