Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kraton® D1160 B (SIS) Linear Triblock Copolymer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Kraton
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® D1160 B (SIS) Linear Triblock Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Kraton D1160 B is a clear linear triblock copolymer based on styrene and isoprene with bound styrene of 18.5% mass. It is supplied from South America in the physical form identified: Kraton D1160 BT - supplied as a porous pellet dusted with talcRegion: South America, Europe, Asia Pacific, North America, and Japan Uses: Kraton D1160 B is used in formulating adhesives, in particular hot melt pressure sensitive adhesives.Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Footwear; and Bitumen ModificationInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ISO 2781
Bulk Density 0.350 g/cc
0.0126 lb/in³
ASTM D1895
Volatiles <= 0.30 %
<= 0.30 %
KM 04
Brookfield Viscosity 700 - 1100 cP
700 - 1100 cP
25% Toluene Solution at 25°C; KM 06
Molecular Weight 168000 - 188000 g/mol
168000 - 188000 g/mol
KM 01
Melt Flow 5.0 - 13 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.0 - 13 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Ash <= 0.50 %
<= 0.50 %
BT; ISO 247
Mechanical Properties Metric English Comments
Hardness, Shore A 48

@Time 30.0 sec
48

@Time 0.00833 hour
Measured on compression molded slabs; ISO 868
Tensile Strength 32.0 MPa
4640 psi
Measured on films cast from a toluene solution; ISO 37
Elongation at Break 1300 %
1300 %
Measured on films cast from a solution in toluene; ISO 37
300% Modulus 0.00190 GPa
0.276 ksi
Measured on films cast from a solution in toluene; ISO 37
Descriptive Properties Value Comments
Content Non-staining phenolic antioxidant
>0.08%, KM 08
Polystyrene
17.4-20.5%, KM 03
Total Extractables
<1.0%, KM 05
Users viewing this material also viewed the following: