Material Notes:
Description: Kraton D1184 A is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows in the grade nomenclature: Kraton D1184 AS - supplied as porous pellets dusted with amorphous silicaKraton D1184 AT - supplied as porous pellets dusted with talcKraton D1184 ASM - supplied as powder dusted with amorphous silicaKraton D1184 AIM - supplied as powder dusted with calcium carbonate for supply to the North American marketRegion: North America, Europe, Asia Pacific, Japan, and South America Uses: Kraton D1184 A polymer is used as a modifier of bitumen in roofing felt compounds, roads and pipe coating. It may also be suitable for use in formulating adhesives, sealants and coatings and in the modification of polymers.Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and RoofingInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 2781
Bulk Density 0.400 g/cc
0.0145 lb/in³
ASTM D 1895 method B
Volatiles <= 0.30 %
<= 0.30 %
KM 04
Viscosity 1000 - 1400 cP
1000 - 1400 cP
25% Toluene Solution at 25°C; KM 06
Melt Flow <= 1.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
<= 1.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Ash <= 0.40 %
<= 0.40 %
AS, AT; ISO 247
2.5 - 5.0 %
2.5 - 5.0 %
ASM, Milled product with silica dusting agent; ISO 247
4.0 - 6.0 %
4.0 - 6.0 %
AIM, Milled product with calcium carbonate dusting agent; ISO 247
Mechanical Properties Metric English Comments
Hardness, Shore A 75

@Time 30.0 sec
75

@Time 0.00833 hour
ISO 868
Tensile Strength 27.0 MPa
3920 psi
ISO 37
Elongation at Break 820 %
820 %
ISO 37
300% Modulus 0.00250 GPa
0.363 ksi
ISO 37
Descriptive Properties Value Comments
Content Antioxidant
>0.14%, Only refers to primary antioxidant content, KM 08
Polystyrene
29-31%, KM 03
Total Extractables
<1.4%, KM 05