Material Notes:
Description: Kraton D4153 E is an oil-extended linear block copolymer based on styrene and butadiene with bound styrene in the neat polymer of 35% mass. It contains 40 phr paraffinic oil which is classified as not hazardous. Information on the CAS and EINECS registry numbers of the paraffinic oil used for this grade is available on request. The product is supplied from Europe in the physical form identified: Kraton D4153 ES - supplied as porous pellets dusted with an amorphous silicaKraton D4153 ESM - supplied as powder dusted with an amorphous silicaRegion: North America, Europe, Asia Pacific, Japan, and South America Uses: Kraton D4153 E is used in formulating compounds for footwear, technical and general purpose applications. It can also be used in formulating adhesives, sealants and coatings and as a modifier of bitumen.Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; and Roads and RoofingInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Bulk Density 0.400 g/cc
0.0145 lb/in³
ASTM D 1895 method B
Volatiles <= 0.30 %
<= 0.30 %
KM 04
Melt Flow 23 - 27 g/10 min

@Load 5.00 kg,
Temperature 200 °C
23 - 27 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Ash 0.15 - 0.35 %
0.15 - 0.35 %
ES; ISO 247
2.5 - 5.0 %
2.5 - 5.0 %
ESM; ISO 247
Mechanical Properties Metric English Comments
Hardness, Shore A 43 - 47

@Time 15.0 sec
43 - 47

@Time 0.00417 hour
Measured on injection molded slabs; ISO 868
Tensile Strength 10.0 MPa
1450 psi
Measured on injection molded slabs; ASTM D412
Elongation at Break 900 %
900 %
Measured on injection molded slabs; ISO 37
300% Modulus 0.00250 GPa
0.363 ksi
Measured on injection molded slab; ISO 37
Abrasion 105
105
[cubic mm], Measured on injection molded slabs; DIN 53516
Descriptive Properties Value Comments
Content Antioxidant
>0.10%, KM 08
Polystyrene
34-36%, KM 03
Total Extractables, Oil
29-32%, KM 05