Material Notes:
Description: Kraton D4270 J is an oil-extended branched block copolymer based on styrene and butadiene, with bound styrene in the neat polymer of 32% mass. It is supplied from Japan in the physical forms identified in the grade nomenclature: D4270 JSP - supplied as dusted pelletsD4270 JS - supplied as dusted crumbRegion: Japan Uses: Kraton D4270 J is used for formulating compounds for footwear and general purpose applications and as a modifier of bitumen.Applications: Bitumen Modification and Compounding and Personal HygieneInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
Volatiles <= 1.0 %

@Temperature 110 °C,
Time 7200 sec
<= 1.0 %

@Temperature 230 °F,
Time 2.00 hour
Melt Flow 10 - 24 g/10 min

@Load 5.00 kg,
Temperature 200 °C
10 - 24 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Ash <= 1.0 %
<= 1.0 %
ISO 247
Mechanical Properties Metric English Comments
Hardness, Shore A 46

@Time 30.0 sec
46

@Time 0.00833 hour
ISO 7619
Tensile Strength 12.0 MPa
1740 psi
ISO 37
Elongation at Break 1100 %
1100 %
ISO 37
300% Modulus 0.00190 GPa
0.276 ksi
ISO 37
Descriptive Properties Value Comments
Content Bound Styrene
32 percent