Material Notes:
Description: Kraton D4433 P is an oiled, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified: Kraton D4433 PT - supplied as a dusted dense pellet Region: Asia Pacific, Europe, Japan, North America, and South AmericaUses: Kraton D4433 P is used as an ingredient in formulating adhesives, sealants and coatings. It may also find use as a modifier of bitumen and polymers.Applications: Adhesives, Sealant and Coatings and Compounding and Personal HygieneNote 1) Primary antioxidant is a non-staining, phenolic antioxidant. The antioxidant package also contains a non-TNPP secondary antioxidant at a target level of 0.2%.Information provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D4025
Volatiles <= 0.70 %
<= 0.70 %
KM 04
Viscosity 380 cP
380 cP
25% Toluene Solution at 25°C; BAM 922
Melt Flow 25 g/10 min

@Load 5.00 kg,
Temperature 200 °C
25 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Ash 0.30 - 0.40 %
0.30 - 0.40 %
Talc; BAM 908
Mechanical Properties Metric English Comments
Hardness, Shore A 29

@Time 10.0 sec
29

@Time 0.00278 hour
Typical values on polymer compression molded at 300°F; ASTM D2240
Tensile Strength 6.21 MPa
901 psi
Measured on films cast from a solution in toluene; ASTM D412
Elongation at Break 1450 %
1450 %
Measured on films cast from a solution in toluene; ASTM D412
300% Modulus 0.00103 GPa
0.149 ksi
Measured on films cast from a solution in toluene; ASTM D412
Chemical Properties Metric English Comments
Diblock Content 20 %
20 %
Descriptive Properties Value Comments
Content Antioxidant
0.08-0.2%, See note 1), KM 08
Oil
21.5-24.5%, KM 05
Polystyrene
20-24%, KM 03
Styrene/Rubber Ratio 22/78