Material Notes:
Description: Kraton D4433 P is an oiled, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified: Kraton D4433 PT - supplied as a dusted dense pelletRegion: Asia Pacific, Europe, Japan, North America, and South America Uses: Kraton D4433 P is used as an ingredient in formulating adhesives, sealants and coatings. It may also find use as a modifier of bitumen and polymers.Applications: Adhesives, Sealant and Coatings; and Compounding and Personal Hygiene
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D4025
Volatiles <= 0.70 %
<= 0.70 %
KM 04
Brookfield Viscosity 380 cP

@Temperature 25.0 °C
380 cP

@Temperature 77.0 °F
25% Toluene solution; BAM 922
Melt Flow 25 g/10 min

@Load 5.00 kg,
Temperature 200 °C
25 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Ash 0.30 - 0.40 %
0.30 - 0.40 %
BAM 908
Mechanical Properties Metric English Comments
Hardness, Shore A 29
29
10 seconds. Typical values on polymer compression molded at 150°C (300°F).; ASTM 2240
Tensile Strength, Ultimate 6.205 MPa
900.0 psi
Typical properties based on film cast from toluene solution.; ASTM D412
Elongation at Break 1450 %
1450 %
Typical properties based on film cast from toluene solution.; ASTM D412
300% Modulus 0.00103 GPa
0.149 ksi
Typical properties based on film cast from toluene solution.; ASTM D412
Chemical Properties Metric English Comments
Diblock Content 20 %
20 %
Descriptive Properties Value Comments
Content Antioxidant
0.06-0.2%, KM 08
Oil
21.5-24.5%, KM 05
Polystyrene
20-24%, KM 03
Styrene / Rubber ratio 22/78