Material Notes:
Description: Kraton FG1924 G is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 13% . It is supplied from North America in the physical form identified: FG1924 GT - supplied as a dusted pelletRegion: Asia Pacific, Europe, Japan, North America, and South America Uses: Kraton FG1924 G is used as a modifier of bitumen or thermoplastics and in compound formulations. It may also find use as an ingredient in formulating adhesives, sealants and coatingsApplications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; and Impact Modification
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Brookfield Viscosity 19000 cP

@Temperature 25.0 °C
19000 cP

@Temperature 77.0 °F
BAM 922
Melt Flow 40 g/10 min

@Load 5.00 kg,
Temperature 230 °C
40 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D412
Mechanical Properties Metric English Comments
Hardness, Shore A 49
49
10 Seconds; ASTM D2240
Tensile Strength, Ultimate 23.44 MPa
3400 psi
ASTM D412
Elongation at Break 750 %
750 %
ASTM D412
Descriptive Properties Value Comments
Content Maleic anhydride, Bound
0.7-1.3%, BAM 1026
Maleic Anhydride, Free
<0.35, OTHR INFWTC
Water
<500 ppm, BAM 1024, At time of packaging
Styrene/Rubber Ratio 13/87