Material Notes:
Description: Kraton G1641 H is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 33%. It is supplied from North America in the physical form identified: Kraton G1641 HU - supplied as an undusted powderKraton G1641 HS - supplied as a dusted powderRegion: Asia Pacific, Europe, Japan, North America, and South AmericaUses: Kraton G1641 H is used in compound formulations and as a modifier of thermoplastics. It may also find use in formulating adhesives, sealants, coatings and modified bitumens.Applications: Compounding and Personal Hygiene; Adhesives, Sealant and Coatings; Impact Modification; Medical; Packaging and Polymod; and Personal CareInformation provided by Kraton®
Physical Properties Metric English Comments
Volatiles <= 0.50 %
<= 0.50 %
KM 04
Viscosity 500 - 850 cP
500 - 850 cP
15% Toluene Solution at 25°C; BAM 922
Mechanical Properties Metric English Comments
Hardness, Shore A 52

@Time 10.0 sec
52

@Time 0.00278 hour
Measured on compression molded slabs; ASTM D2240
Tensile Strength >= 17.2 MPa
>= 2490 psi
Measured on solution cast film from toluene; BAM 1245
Elongation at Break >= 800 %
>= 800 %
Measured on solution cast film from toluene; BAM 1245
300% Modulus 0.00434 GPa
0.629 ksi
Measured on solution cast film from toluene; BAM 1245
Descriptive Properties Value Comments
Content Non-staining phenolic antioxidant
0.03-0.1%, KM 08
Polystyrene
32.3-33.7%, Measured on polymer before hydrogenation, KM 03
Total Extractables
<1.6%, KM 05